CM350LN | Impact Copolymer | Nucleated. Antistat. | 35 g/10 min | 160,000 psi | 3,100 psi | 7.2% | 2.3 ft-lb/in | 96°C |
CM200LN | Impact Copolymer | UL 94 HB, Nucleated. Antistat., No-Break Izod Impact | 20 g/10 min | 137,000 psi | 2,850 psi | 9.5% | No Break | 92°C |
CM005 | Impact Copolymer | Excellent Impact Properties in RT & -30°C, USP Class VI, GMW17178, Stellantis MS-DB-500 CPN4002 Color: Natural | 0.45 g/10 min | 175,000 psi | 3,650 psi | 15% | No Break | 81ºC |
CH350 | Homopolymer | Reactor Grade, DMF Listed, UL 94 HB | 35 g/10 min | 240,000 psi | 5,400 psi | 7.5% | 0.5 ft-lb/in | 101ºC |
CH040 | Homopolymer | NSF 51 Listed, High Crystallinity | 4 g/10 min | 255,000 psi | 5,200 psi | 8% | 0.8 ft-lb/in | 100ºC |
CH120LN | Homopolymer | UL 94 HB, DMF Listed, USP Class VI, USP <661.1> | 12 g/10 min | 280,000 psi | 5,250 psi | 7% | 1 ft-lb/in | 119°C |
CH005 | Homopolymer | NSF 51 Listed, UL 94 HB, USP Class VI | 0.5 g/10 min | 230,000 psi | 5,100 psi | 11% | 1.5 ft-lb/in | 94°C |
CH120 | Homopolymer | Barefoot, UL 94 HB | 12 g/10 min | 240,000 psi | Tensile Strength @ Yield : 5,000 psi | 8% | 0.7 ft-lb/in | 101°C |